Send inquiry
White latex Wood Veneer Lamination Glue
Name: White Glue
Features:
good initial adhesion, quick drying
Application:
Widely used in wood lamination, stick a wood skin, paper.
Operation method:
1. Wood surface processing: Make the wood surface free of oil, dirt andother impurities. The bonding surface must level off, so the adhesive canfully contact.
2. The rate of water in wood should be controlled in 8-15%, too high or
low will affect the bonding quality.
3. The open time: 2-5 minutes before the adhesive solution became the film. The shorter the better. Suitable amount of coating should be uniform. The glue quantity is 180-180 grams per square meter.
4. Pressure time: Cold pressing 2-8 hours, depending on the water content and temperature conditions of Base material. When pressuring, the pressure should be enough and which should be pressurized for 2
Hours. To achieve better bonding effect, it is best to 24 hours after pressure relief for processing.
5. For some special materials, i can be used mixed with some resin to enhance the bonding effect.
Operation method:
1. Wood surface processing: Make the wood surface free of oil, dirt andother impurities. The bonding surface must level off, so the adhesive canfully contact.
2. The rate of water in wood should be controlled in 8-15%, too high or
low will affect the bonding quality.
3. The open time: 2-5 minutes before the adhesive solution became the film. The shorter the better. Suitable amount of coating should be uniform. The glue quantity is 180-180 grams per square meter.
4. Pressure time: Cold pressing 2-8 hours, depending on the water content and temperature conditions of Base material. When pressuring, the pressure should be enough and which should be pressurized for 2
Hours. To achieve better bonding effect, it is best to 24 hours after pressure relief for processing.
5. For some special materials, i can be used mixed with some resin to enhance the bonding effect.
Name: White Glue
Product Specification |
Wood Veneer Lamination Glue |
Type |
DF-225 |
Appearance |
white adhesive liquid |
Viscosity | 30000-50000mpa.s |
Solid conten | 22%(adjustable) |
PH value | 7.0-8.0 |
Packing |
Using 25 kg or 50kg plastic drum |
Features |
Good initial adhesion, quick drying |
Application | Widely used in wood lamination, stick a wood skin, paper |
Product Specification |
Wood Veneer Lamination Glue |
Type |
DF-2010 |
Appearance |
white adhesive liquid |
Viscosity | 10000-20000mpa.s |
Solid conten | 26%(adjustable) |
PH value | 4.0-6.0 |
Packing |
Using 25 kg or 50kg plastic drum |
Features |
Good initial adhesion, quick drying |
Application | Widely used in wood lamination, stick a wood skin, paper |
Product Specification |
Cork Board Glue |
Type |
AE-5005 Water-based |
Appearance |
Milky white liquid |
Viscosity | 8000-10000mpa.s |
Solid conten | 47%(adjustable) |
PH value | 6.5-8.5 |
Packing |
Using 25 kg or 50kg plastic drum |
Features |
The bond strength of bonding area is veryhigh. The adhesive has good heat resistance andsolvent resistance. |
Application |
Widely used for soft wood |
Features:
good initial adhesion, quick drying
Application:
Widely used in wood lamination, stick a wood skin, paper.
Operation method:
1. Wood surface processing: Make the wood surface free of oil, dirt andother impurities. The bonding surface must level off, so the adhesive canfully contact.
2. The rate of water in wood should be controlled in 8-15%, too high or
low will affect the bonding quality.
3. The open time: 2-5 minutes before the adhesive solution became the film. The shorter the better. Suitable amount of coating should be uniform. The glue quantity is 180-180 grams per square meter.
4. Pressure time: Cold pressing 2-8 hours, depending on the water content and temperature conditions of Base material. When pressuring, the pressure should be enough and which should be pressurized for 2
Hours. To achieve better bonding effect, it is best to 24 hours after pressure relief for processing.
5. For some special materials, i can be used mixed with some resin to enhance the bonding effect.
Operation method:
1. Wood surface processing: Make the wood surface free of oil, dirt andother impurities. The bonding surface must level off, so the adhesive canfully contact.
2. The rate of water in wood should be controlled in 8-15%, too high or
low will affect the bonding quality.
3. The open time: 2-5 minutes before the adhesive solution became the film. The shorter the better. Suitable amount of coating should be uniform. The glue quantity is 180-180 grams per square meter.
4. Pressure time: Cold pressing 2-8 hours, depending on the water content and temperature conditions of Base material. When pressuring, the pressure should be enough and which should be pressurized for 2
Hours. To achieve better bonding effect, it is best to 24 hours after pressure relief for processing.
5. For some special materials, i can be used mixed with some resin to enhance the bonding effect.
Environmental Capability:
Our water-based acrylic glue does not append formaldehyde, benzene and heavy metal, meet the standard as follows:
1) Meet EU EN71-3& USA ASTM F963 standard
2) Meet EU & China ROHS & 16 items of phthalate standard.
3) Meet EU 94/62/EC Packing Directive / CONGE packing material standard.
FAQ:
ShanDong HanShiFu Adhesive Co.Ltd
Phone:+86 15153909617
Add: Hedong district, Linyi city, ShanDong, China